DSpace Repository

Investigate the Temperature Effects on Curing of Reactive Powder Concrete Containing Silica

Show simple item record

dc.contributor.author Sonkusare, Hemantkumar G.
dc.contributor.author Pawade, Prashant Y.
dc.date.accessioned 2025-01-01T07:44:08Z
dc.date.available 2025-01-01T07:44:08Z
dc.date.issued 2021
dc.identifier.citation Sonkusare, H.G., Pawade, P.Y. (2021). Investigate the Temperature Effects on Curing of Reactive Powder Concrete Containing Silica. Advances in Civil Engineering and Infrastructural Development. Lecture Notes in Civil Engineering, vol 87. Springer, Singapore. https://doi.org/10.1007/978-981-15-6463-5_71 en_US
dc.identifier.uri http://10.9.150.37:8080/dspace//handle/atmiyauni/2155
dc.description.abstract There is a burgeoning use of reactive powder concrete unsettled to the outstanding mechanical properties and resilience. Reactive powder concrete structural elements can resist chemical paroxysm, impact loading from vehicles and vessels, and sudden kinetic loading due to earthquakes. In addition, the lower maintenance requirements result in significant economic detriment. Moreover, in the composition of reactive powder concrete, a fractional substitution of cement by silica fume (which is a waste by-product of silicon alloy) results in less cement consumption (and hence less greenhouse gas emission). In this experimental investigation study, the material performance of reactive powder concrete (RPC) with two different curing techniques, normal water curing of 25 °C and accelerated steam curing at 60 °C, and 60% relative humidity, was studied experimentally. This paper also remits the investigation, application, and different preparation of silica fume in reactive powder concrete at transformed temperature. The silica fume was substituted with the cement and the dosage which bequeathed the maximum strength was used for further addition of silica sand and steel fibers. Steam curing is effective process to achieve high early strength, and in this narrative, the compressive strength at the age of 3, 7, and 28 days was determined for further compared with normal cured water. Also find split tensile test to see the performance of concrete cylinder under tension. To reduce the water content, super plasticizer may be used as an admixture. Thus, results are interpreted for different combination to achieve maximum compressive stress as well as tensile stress. en_US
dc.language.iso en en_US
dc.publisher Advances in Civil Engineering and Infrastructural Development. Lecture Notes in Civil Engineering en_US
dc.relation.ispartofseries 87;
dc.title Investigate the Temperature Effects on Curing of Reactive Powder Concrete Containing Silica en_US
dc.type Article en_US