DSpace Repository

Degradation efficiency of malachite green dye by LaCO0.8Cu0.2O3 perovskite oxide under natural and UV condition

Show simple item record

dc.contributor.author khakhariya, Sahil
dc.contributor.author Kher, David
dc.contributor.author Khunt, Meet
dc.contributor.author Malakiya, Meet
dc.date.accessioned 2023-05-09T05:52:12Z
dc.date.available 2023-05-09T05:52:12Z
dc.date.issued 2023
dc.identifier.citation Khakhariya, S., Kher, D., Khunt, M., & Malakiya, M. (2023). Degradation efficiency of malachite green dye by LaCO0.8Cu0.2O3 perovskite oxide under natural and UV condition. Department Of Industrial Chemistry Faculty Of Science (Fos) Atmiya University en_US
dc.identifier.uri http://10.9.150.37:8080/dspace//handle/atmiyauni/893
dc.description.abstract Perovskite are the catalytic material having the general formula of ABO3 and can be prepared by various synthetic methods such as Co-precipitation method, Citrate method, Ball mill method, Sol-gel method etc. They are being applied in many areas of current development because of their optical, magnetic, electronic and ferroelectric properties. General uses of Perovskite nano-particles have been in adsorbents for waste water treatment, fuel cells, drug delivery and air pollution controller. The ultimate goal of the wastewater treatment is to provide the protection of human health and environmental aspect. The interest in these catalysts has been revitalized in the past ten years by the introduction of the concept of catalyst generatability of Perovskite Catalyst, which is in principle well. en_US
dc.language.iso en en_US
dc.title Degradation efficiency of malachite green dye by LaCO0.8Cu0.2O3 perovskite oxide under natural and UV condition en_US
dc.type Thesis en_US


Files in this item

This item appears in the following Collection(s)

Show simple item record

Search DSpace


Advanced Search

Browse

My Account